Report

PHYSICAL TEST REPORT

Sr:No Test Result Unit Standard Institute
1 Tensile Strength 331.5 kg/cm2 ASTM D 638 CIPET-Ahmedabad
2 Elongation at break 11 % ASTM D 638
3 Density 1.52 Gm/cc ASTM D 792
4 Vst AT 1 KG. LOAD 86.6 0C ASTM D 1525
5 Flexural strength 622.3 kg/cm2 ASTM D 790
6 Flexural modulus 21850 kg/cm2 ASTM D 790
7 Izod Impact strength 41 J/m ASTM D 256
8 Water Absorption 0.16 % ASTM D 570
9 Rockwell Hardness ® Scale 70 --- ASTM D 785
10 HDT AT 66 psi 72.4 0C ASTM D 648
11 HDPT AT 264 psi 64.7 0C ASTM D 648
12 Limiting Oxygen Index 31 % ASTM D 2863
13 Flammability VO --- UL-94
14 Long Term Heat Resistance No Effect --- ASTM D 794 Alekh Plastics Testing Center-Ahemdabad
15 Weight Loss ZERO(@2000C) --- --- SICRAT - V.V.Nagar

CHEMICAL TEST REPORTS

Sr:No Test Result Unit Standard Institute
1 Chemical Resistance( in 18% HCL) No Effect --- ASTM D 543 Alekh Plastics Testing Center-Ahmedabad
2 Chemical Resistance( in 20% NaOH) No Effect --- ASTM D 543
3 Chemical Resistance( in saturated solution) No Effect --- ASTM D 543